Ni-Span-C Alloy 902, N09902, Nickel Alloy Spring Wire

Ni-Span-C Alloy 902, N09902, Nickel Alloy Spring Wire
Ni-Span-C Alloy 902, N09902, Nickel Alloy Spring Wire

Large Image :  Ni-Span-C Alloy 902, N09902, Nickel Alloy Spring Wire

Product Details:
Place of Origin: CHINA
Brand Name: fushun
Certification: ISO NQA
Model Number: 902
Payment & Shipping Terms:
Minimum Order Quantity: 1KG
Delivery Time: 1
Payment Terms: L/C, T/T, D/P, D/A

Ni-Span-C Alloy 902, N09902, Nickel Alloy Spring Wire

Description
Material: Nickel Alloy Application: Spring

Ni-Span-C Alloy 902, N09902, Nickel Alloy Spring Wire

A precipitation hardenable Nickel-Iron-Chromium alloy having outstanding controllable thermoelastic coefficient characteristics and excellent oxidation resistance in high temperature atmospheres. The alloy can be processed to have a constant modulus of elasticity at temperatures ranging from -45 to +65°C (-50 to +150°F).

 

Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped

 

Key Features

Outstanding controllable thermoelastic coefficient characteristics.

Can be processed to have constant modulus of elasticity from from -45 to +65ºC (-50 to +150ºF).

Good for springs in watches and weighing equipment.

Age hardenable.

 

Typical Applications

Springs in precise applications, such as

watches

weighing machines

 

Designations

UNS N09902

AWS 080

 

Specifications

AMS 5225

AMS 5221

HS 261

 

Chemical Composition

Element Min % Max %
C 0.06
Mn 0.8
Si 1
P 0.04
S 0.04
Cr 4.9 5.75
Ni+Co 41 43.5
Ti 2.2 2.75
Al 0.3 0.8
Cr+(Ti-4xC) 7.1 8.1
Co 1
Fe Bal Bal

 

Physical Properties

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.05 g/cm³ 1480 °C 7.6 μm/m °C (20 – 100 °C) 62 – 69 kN/mm² 165 – 200 kN/mm²
0.291 lb/in³ 2700 °F 4.2 x 10-6 in/in °F (70 – 212 °F) 8993 – 10008 ksi 23932 – 29008 ksi

 

Heat treatment

Condition Type Temperature Time Cooling
Spring Temper – For good all round properties Age Harden 650 °C (1200 °F) 2 Hr Air
Spring Temper – For max stability Stress Equalise
Age Harden
400 °C (750 °F)
650 °C (1200 °F)
2 Hr
2 Hr
Air
Air
Spring Temper – For minimum hysterisis & low thermoelastic coefficient Stress Equalise 400 °C (750 °F) 2 Hr Air

 

Mechanical Properties

Annealed Approx. tensile strength <800 N/mm² <116 ksi
Approx. operating temperature (for constant modulus applications) -45 to +65 °C -50 to +150 °F
Spring Tempered Approx. tensile strength 900 – 1100 N/mm² 131 – 159 ksi
Approx. operating temperature (for constant modulus applications) -45 to +65 °C -50 to +150 °F
Spring Temper + Aged Approx. tensile strength 1300 – 1500 N/mm² 189 – 218 ksi
Approx. operating temperature (for constant modulus applications) -45 to +65 °C -50 to +150 °F

 